The standard every wall is built to
Updated 16 November 2026
Most problems in a boundary wall are hidden once it is finished: a shallow footing, steel lying on the soil, bricks laid with gaps in the mortar. Plaster covers all of it. So we check each stage before the next one covers it up. The same standard is written into our agreement with the building crew, which is led by a builder with 20 years' experience.
The five checks
The crew does not move on to the next stage until we have checked the one before.
- Setting out and the open trench, before any concrete is poured. The wall is on the agreed line and inside your boundary.
- The steel in the trench, before it is covered (walls on open ground).
- The first courses on the footing, including the waterproofed mortar.
- The finished brickwork, before plastering starts. This is where gaps in the mortar are found, because plaster hides them.
- The finished wall, with you. We walk it together before the final payment.

What we measure
We check with a spirit level, a string line, a tape measure and a 2 m straightedge.
| Check | Our standard |
|---|---|
| Position | On the line agreed with you at the site visit, and inside your boundary. |
| Foundation | A concrete strip footing on firm, undisturbed ground. On open ground, the steel bars are lifted off the soil and fully covered by concrete. |
| Upright | No more than 10 mm out from top to bottom, on the wall and on every pillar face. |
| Straight | No more than 10 mm off a string line in any 6 m. |
| Level | Courses level along the wall. On sloping ground the wall steps down evenly, with the steps at pillars. |
| Mortar joints | Every brick fully bedded in mortar: full joints under each brick and at both ends, and the gap between the two skins filled. No dry joints or holes. Joints about 10 mm thick and even. |
| Neat brickwork | Whole bricks laid in a proper bond, even where the wall will be plastered. No cracked or broken bricks on show. Face brick is mixed from several pallets so the colour is even, and cleaned the same day. |
| Strength | Brickforce across both skins every few courses and under the top course. Pillars built into the wall, not added on. |
| Plaster | No gap of more than 5 mm under a 2 m straightedge. Sharp, straight corners. The top sloped so that rain runs off. No hollow or loose patches. |
| Curing | The footing and the plaster are kept damp for at least 3 days so they reach full strength. |
| Your property | The site is cleaned at the end of every day, rubble is kept in one place, and nothing is left behind. |
If something is not right
Work that does not meet the standard is fixed or rebuilt before the next stage starts, and before we ask you for the final payment. You do not pay for the rework. Our building crew's final payment is released only after the wall has passed.
After the wall is finished
Our workmanship is guaranteed for 6 months after the wall is finished. If a fault from our workmanship shows in that time, such as a crack from poor work, a wall that is out of plumb or plaster coming loose, we come back and fix it. Fine hairline cracks in plaster are normal as it dries and are not a fault.
How you pay
- Deposit when you accept the quote. It pays for your materials (about half the price), which are delivered to your property.
- Stage payment when the brickwork is up.
- Final payment after you have walked the finished wall with us.
Every payment goes to We Build Walls by bank transfer, against a written request. Never pay the building crew.